Black Silicon Carbide 54C. Grinding Powder F120

Black Silicon Carbide 54C. Grinding Powder F120

Silicon carbide black 53C (54C) is an artificial abrasive of high strength obtained by melting muassanite in a graphite electric furnace.
お問い合わせを送る
説明
技術的なパラメーター
Black Silicon Carbide 54C. Grinding Powder F120 Description

 

Silicon carbide black 53C (54C) is an artificial abrasive of high strength, obtained by melting muassanite in a graphite electric furnace.


- SiC approximately 98%.
- The remaining part is occupied by other minerals.

- Hard.
- Refractory - melting point is approximately 2500 degree .
- Heat conductive.
- High cutting ability.
- Special electrically conductive properties.

 

product-600-500

 

 

 

The Specification Of Black Silicon Carbide 54C. Grinding Powder F120

 

9.15
2250 degree
1900 degree
3.2-3.4g/cm3
2840-3320kg/mm2

 

product-450-450product-600-500

 

 

 

 



 